INCOLOY 800HT / NICKEL ALLOY 800HT / UNS N08811
Ni:30~35
Cr:19~23
Fe:39.5~46
Mn:1.5 max.
Co:2 max
Al:0.25~0.6 max
Ti:0.25~0.6 max
Si:1max
C:0.06 - 0.1max
Cu:0.75max
S:0.015max
-Tensile Strength: (MPa) = 450 MPa min
-Yield Strength: (MPa) = 170 MPa min
-Elongation (%) = 30% min
-Hardness: (HB) = 125 max
-Alloy 800HT
-WNr DIN EN 1.4959
-UNS N08811
-DIN EN X8NiCrAlTi32-21
Seamless Pipes -B407
Seamless Tubes -B407, B163
Seamless Pipes - SB 407
Seamless Tubes - SB 407, SB 163